Keluli Karbon Tinggi Elektrod manual E9818-G Pembuatan pematerian
KOMPONEN KIMIA:
ALOI(berat%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu | V |
PERATURAN GB/T | - | ≥1.00 | ≥0.80 | ≥0.30 | ≥0.50 | ≥0.20 | - | - | ≥0.20 | ≥0.10 |
PERATURAN AWS | - | - | - | - | - | - | - | - | - | - |
NILAI CONTOH | 0.050 | 1.50 | 0.27 | 0.83 | 3.35 | 0.72 | 0.005 | 0.004 | 0.018 | 0.004 |
HARTA MEKANIKAL:
HARTANAH | KEKUATAN HASIL (MPa) | KEKUATAN LANJUTAN(MPa) | HEATTREAMENT℃xh | NILAI IMPAK J/℃ | PEMANTAPAN(%) | |||||
PERATURAN GB/T | - | - | - | - | - | |||||
PERATURAN AWS | - | - | - | - | - | |||||
NILAI CONTOH | 915 | 992 | - | 65/-20 | 16 |
PARAMETER KIMPALAN YANG DISARANKAN:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||||
ELEKTRIK (Amp) | H/W | 80-110 | 100-130 | 130-180 | 180-230 | |||||
O/W | 50-80 | 90-120 | 130-160 | - |
980Mpa kekuatan super tinggi serbuk ferrohidrogen rendah jenis elektrod keluli aloi rendah.
Arka stabil, percikan kecil, penyingkiran sanga yang baik
Prestasi kimpalan semua kedudukan yang sangat baik, keliatan suhu rendah yang baik, rintangan retak dan keliatan hentaman suhu rendah.
KOMPONEN KIMIA:
ALOI(berat%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu | V |
PERATURAN GB/T | - | ≥1.00 | ≥0.80 | ≥0.30 | ≥0.50 | ≥0.20 | - | - | ≥0.20 | ≥0.10 |
PERATURAN AWS | - | - | - | - | - | - | - | - | - | - |
NILAI CONTOH | 0.050 | 1.50 | 0.27 | 0.83 | 3.35 | 0.72 | 0.005 | 0.004 | 0.018 | 0.004 |
HARTA MEKANIKAL:
HARTANAH | KEKUATAN HASIL (MPa) | KEKUATAN LANJUTAN(MPa) | HEATTREAMENT℃xh | NILAI IMPAK J/℃ | PEMANTAPAN(%) | |||||
PERATURAN GB/T | - | - | - | - | - | |||||
PERATURAN AWS | - | - | - | - | - | |||||
NILAI CONTOH | 915 | 992 | - | 65/-20 | 16 |
PARAMETER KIMPALAN YANG DISARANKAN:
SPESIFIKASI DIAMETER (mm) | 2.6*350 | 3.2*350 | 4.0*400 | 5.0*400 | ||||||
ELEKTRIK (Amp) | H/W | 80-110 | 100-130 | 130-180 | 180-230 | |||||
O/W | 50-80 | 90-120 | 130-160 | - |